42CrMoS4 Tensile Tests Fraunhofer IWM
Data of tensile tests, round specimen, B5x25. Performed at room temperature. Material quenched and tempered, austenitizing temperature 850 °C. -
TEM CuZn23Si2.5 IMWS
TEM results (image and metafile) of CuZn23Si2.5